闊恒興旺貿(mào)易(南寧市分公司)全體員工向關(guān)心和支持我們的各級(jí)領(lǐng)導(dǎo)和各界朋友表示z u i誠(chéng)摯的謝意! 在 熱鍍鋅工字鋼市場(chǎng)競(jìng)爭(zhēng)日趨激烈的今天,闊恒興旺貿(mào)易(南寧市分公司)勵(lì)精圖治,奮發(fā)自強(qiáng),為振興民族 熱鍍鋅工字鋼和廣西南寧經(jīng)濟(jì)而奮斗不息, 公司經(jīng)理攜全體員工恭候各地新老賓客光臨本 熱鍍鋅工字鋼生產(chǎn)企業(yè),實(shí)地考察、指導(dǎo)工作、增進(jìn)了解!


T1的化學(xué)成份Cu+Ag99.95%,P0.001%,Bi0.001%,Sb0.002%,As0.002%,F(xiàn)e0.005%,Ni0.002%,Pb0.003%,Sn0.002%,S0.005%,Zn0.005%,O0.02%。
T2的化學(xué)成份Cu+Ag99.95%,Bi0.001%,Sb0.002%,As0.002%,F(xiàn)e0.005%,Pb0.005%,S0.005%。
導(dǎo)熱率(λ)384/W·(m·K)-1
比熱熔(C) 0.394/kj·(kg·K)-1
紫銅管標(biāo)稱直徑(mm)8,10,15,20,25,32,40,50,65,80,100,125,150,in 1/4 3/8 1/2 5/8 3/41 1 1/4 1 1/2 2 2 1/2 3 3 1/2 4 5 6
平均外徑(mm)9.52,12.7,15.88,19.05,22.22,28.58,34.92,41.28,53.98,66.68,79.38,92.08,104.78,130.18,155.58K級(jí)0.89,1.24,1.24,1.24,1.65,1.65,1.65,1.83,2.11,2.41,2.77,3.05,3.40,4.06,4.78
壁厚(mm)L級(jí)0.76,0.89,1.02,1.07,1.14,1.27,1.40,1.52,1.78,2.03,2.29,2.54,2.79,3.18,3.56 M級(jí)0.64,0.71,0.81,0.89,1.07,1.24,1.47,1.65,1.83,2.11,2.41,2.77,3.10


焊接性能優(yōu)勢(shì):易于錫焊、銅焊,也能進(jìn)行氣體保護(hù)焊、閃光焊、電子束焊和氣焊,但不宜進(jìn)行接觸點(diǎn)對(duì)焊和埋弧焊。
可切削性(HPb63-3的切削性為)/%:20
2、磷脫氧銅管的工藝優(yōu)勢(shì):
熔煉與鑄造工藝優(yōu)勢(shì):使用工頻有芯感應(yīng)電爐熔煉。高溫下純銅吸氣性強(qiáng),熔煉時(shí)應(yīng)盡量減少氣體來(lái)源,并使用經(jīng)煅燒過(guò)的木炭作熔劑,也可用磷做脫氧劑,澆鑄過(guò)程在氮?dú)獗Wo(hù)或復(fù)蓋煙灰下進(jìn)行,鑄造溫度為1150-1180℃。
成形性能優(yōu)勢(shì):有優(yōu)良的冷、熱加工性能,可以進(jìn)行精沖、拉伸、墩鉚、擠壓、深沖、彎曲和旋壓等。熱加工溫度為800-900℃。
焊接性能優(yōu)勢(shì):易于熔釬焊、氣體保護(hù)焊但不宜進(jìn)行電阻對(duì)縫焊。
可切削性(HPb63-3的切削性為)/%:20
3、磷脫氧銅管的工藝優(yōu)勢(shì):
熔煉與鑄造工藝優(yōu)勢(shì):使用公頻有芯感應(yīng)電爐熔煉,原料選用Wcu>99.97%及Wzn
成形性能優(yōu)勢(shì):有極好的冷、熱加工性能,能用各種傳統(tǒng)的加工工藝加工,如拉伸、壓延、擠壓、彎曲、沖壓、剪切、鐓煅、旋煅、滾花、纏繞、旋壓、螺紋軋制等??慑懶詭缀?,為鍛造黃銅的65%,熱加工溫度為800-900℃。
焊接性能優(yōu)勢(shì):易于熔焊、釬焊、氣體保護(hù)焊但不宜進(jìn)行金屬弧焊和大多數(shù)電阻焊
可切削性(HPb63-3的切削性為)/%:20
紫銅管的缺點(diǎn)
就紫銅管而言,生產(chǎn)成本高,價(jià)位高是它的 缺點(diǎn),與其他管件相比,紫銅管的成本要高出很多,而且銅管接口處連接對(duì)施工的工藝水平要求較高。